CURRENT LOCATION:HOME >> TECHNICAL SERVICE >>  Technical Q & A

How many kinds of magnetic scars are caused by nondefective?

1. The local cold is hardened, and the magnetic mark caused by the magnetic variation of the material is accumulated; 

2. Magnetic powder accumulation at the interface of two different materials; 

3. Segregation of carbide layers; 

4. Variation of the section size of the parts; 

5. Excessive magnetic current caused by the metal flow line; 

6. Speckle marks caused by an uncleanness or grease on the surface of the workpiece.